Blikkoper geleidende foelieband vir EMI-afskerming
Plek van herkoms: KwaZulu-Natal, China
Brand Naam: Xinst
Model nommer: 6970CU
Materiaal: Tin + Cu
Feature: hittebestande
Gebruik: Masking
Adhesive: Akriel
gom kant: Double Sided
Adhesive Tipe: druk sensitiewe
Design Printing: Geen Printing
Kleur: Koper
Dikte (mm): 0,08
Toepassing: Herstel vir die afskerming van seinkabel of FFC
Blikvormige koper geleidende foelieband Produkbeskrywing
Tin-plated-copper-conductive-foil-tape consists of an embossed deadsoft tin-plated copper foil backing and an aggressive pressure-sensitve acrylic adhesive. The edgs of the embossed pattern pressed into the foil cut through the adhesive layer to establish reliable metal-to-metal contact between the backing and the application substrate.
Kenmerke:
• Goeie elektriese geleidingsvermoë vanaf die basismateriaal deur die oppervlak van viskose tot foeliesubstraat.
• Met goeie afskermeffek.
Ons mededingende voordele in die fabriek:
Well Competitive Prices and High Quality Control.
Prompt Delivery.
Earth-friendly Products.
In a Variety of Design.
Small Order Acceptable.
OEM Accepted.
Roll Size: 3″ paper or plastic core;tape width: 2mm -1200mm; standard width: 1200mm, standard length: 50M.
OEM Size: Special length, thickness or combinations can be supplied per customer’s request. Products can be supplied in roll, tape, sheets or shapes per customer’s request. Only you provide the CAD drawing, we can die cut any size for you.
Houdbaarheid: Om die beste werkverrigting te behaal, gebruik hierdie produk binne 12 maande vanaf afleweringsdatum en bewaar dit onder normale omstandighede van 60 ºC tot 80 ºF (16 ºC tot 27 ºC) en 40 tot 60% RH in die oorspronklike karton.
As die mylar-band van die troeteldier-isolasie-transformator aan u vereistes voldoen, kan u die kwaliteit produkte wat in China vervaardig word by ons professionele vervaardigers en verskaffers in China koop. Ons is toegerus met 'n produktiewe fabriek tot u diens.
Double Tin Plated Copper Conductive Foil Tape Applications:
• Used for high-end electronic equipment, components of the grounding and EMI shielding, the tin on the plating layer has good weld-ability, and high oxidation and corrosion resistance.
Double Tin Plated Copper Conductive Foil Tape Spesifikasies:
Part No. | Kleur | Backing | Total Thickness (um) | The melting point temperature of tin plating layer | Adhesion (g/25mm) |
6970CU | Sliver | Tin+Cu | 70±5 | >232℃ | 800±100 |